E6015 Welding Electrode
Standard: GB/T 5117-1995 E4315 (J427), AWS E6015
Diameter: 2.5*300 mm,3.2*350 mm,4.0*400 mm and 5.0*400 mm
Packing details: 5 kgs/plastic bag in a color box, 20kgs/carton, 1 ton in a pallet
Specification: It is a kind of carbon steel electrode with low-hydrogen natrium type coating. DCRP (Direct Current Reversed Polarity). All-position welding. The deposited metal has excellent mechanical properties, crack-resistance and good low temperature impact toughness.
Application: Used for welding key steel structures under pressure and loads, low-carbon steel thick plate structures and low-alloy steel structures, such as machinery, shipbuilding, bridges, pressure vessels, etc.
Chemical composition of deposited metal (%)
Chemical composition |
C |
Mn |
Si |
S |
P |
Cr |
Ni |
Mo |
V |
Typical |
0.067 |
0.89 |
0.49 |
0.008 |
0.020 |
0.06 |
0.02 |
<0.001 |
0.01 |
Specification |
≤0.12 |
≤1.25 |
≤0.90 |
≤0.035 |
≤0.040 |
≤0.20 |
≤0.30 |
≤0.30 |
≤0.08 |
Mechanical properties of deposited metal
Mechanical properties |
Yield Point |
Tensile Strength |
Elongation |
Charpy V-notch Impact Value(J) |
|
Typical |
380 |
465 |
29 |
-30℃ |
120 |
Specification |
≥330 |
≥420 |
≥22 |
≥27 |
Instructions:
1.The electrodes must be baked under 300~350℃ for an hour before welding and used as soon as baking is completed.
2. The stains on the weldments, such as rust, oil stains, moisture, etc., must be cleared away before welding.
3. When welding, short arc must be used and stringer bead is suitable.
4.This kind of electrodes can also be used in AC welders, but the welding performance will be a little worse than that of the electrodes used in DC welders.
Mobile:+86-13587457912
Tel:+86-577-62511132
Email:info@tyuelec.com